Material: | Neodymium And Iron And Boron | Color: | Silver |
---|---|---|---|
Particle Size: | 80-200um | Br: | 8.5-8.8kGS |
Hcb: | 6-6.5kGs | Hcj: | 9-10kOe |
BH: | 14-14.7MGOe | Working Temperature: | -45 °c——150 °c |
High Light: | MRI scanner magnetic fingerprint powder,Rare Earth Magnetic fingerprint powder,Rare Earth powdered magnets |
MGT-14-09 Rare-Earth Magnet
Rare Earth Magnetic powder type
1) NdFeB powder can be used in the automotive industry, office automation, and automobiles. DC brushed motor. Multipolar stepper and spindle motor applications. Magnetic coatings, magnetic printable substrates, magnetic films, medical diagnostics and therapy, video tapes, copy toner, fingerprint recognition, sensors, fuel injectors, permanent magnets, nanoscale fluid seals, electric toys and magneto-curable products.
2) Samarium Cobalt Powder Samarium Cobalt Powder Samarium Cobalt Magnetic Powder Rare Earth Magnetic Powder Used to produce polymer-bonded samarium cobalt magnets by compression molding.
Production List | ||||||||||||
Series | 0806 | 10-8 | 1208 | 1309 | 1309A | 1412 | 1507 | 1509 | 1510 | 1610 | 1609D | |
magnetic Powder VSM |
Br | 7.00~7.20 | 7.60~7.75 | 8.10~8.30 | 8.40~8.55 | 8.5-8.7 | 8.45-8.65 | 9.2-9.45 | 8.85-9.1 | 8.85-9.1 | 9.05-9.2 | 8.85-9.2 |
kGs | ||||||||||||
Hcj | 5.00~7.50 | 7.80~8.80 | 8.00~8.80 | 9.00~9.80 | 9-9.8 | 12-12.7 | 6.8-7.8 | 9.2-9.8 | 10-10.8 | 9.3-10.1 | 9.2-9.8 | |
kOe | ||||||||||||
Hcb | 4.30-5.00 | 5.20~5.60 | 5.80~6.30 | 6.20~6.80 | 6.2-6.8 | 6.7-7.2 | 5.5-6 | 6.4-6.9 | 6.4-6.9 | 6.7-7.2 | 6.7-7.2 | |
kOe | ||||||||||||
(BH)max | 8.80-9.30 | 11.70~12.10 | 13.00~13.80 | 14.20~14.80 | 14.2-15.1 | 14.4-15.2 | 15-16 | 15.5-16.3 | 15.5-16.3 | 16.5-17.5 | 16.5-17.5 | |
MGOe | ||||||||||||
magnet D10*T10mm |
Br | 5.50~5.90 | 6.00~6.15 | 6.35~6.50 | 6.60~6.80 | 6.6-6.9 | 6.7-6.8 | 7.3-7.5 | 6.9-7 | 6.9-7 | 7.05-7.15 | 7.05-7.15 |
kGs | ||||||||||||
Hcj | 5.00~7.50 | 7.80~8.80 | 8.00~8.80 | 9.00~9.80 | 9-9.8 | 12-12.7 | 6.8-7.8 | 9.2-9.8 | 10-10.8 | 9.3-10.1 | 9.2-9.8 | |
kOe | ||||||||||||
Hcb | 3.80~4.40 | 4.80~5.10 | 5.10~5.40 | 5.40~5.80 | 5.4-5.8 | 5.7-5.9 | 5.3-5.5 | 5.7-6 | 5.7-6 | 5.7-6.2 | 5.8-6.2 | |
kOe | ||||||||||||
(BH)max | 6.00~6.40 | 7.40~7.70 | 8.30~8.70 | 8.90~9.30 | 9-9.4 | 9.6-9.8 | 10.3-10.5 | 9.9-10.3 | 9.9-10.3 | 10.2-10.6 | 10.2-10.6 | |
MGOe |
The process
The molten NdFeB alloy is sprayed onto the cooling rollers at a certain speed and instantly solidifies to form a thin strip of 0.02-0.05mm thickness. During the rapid cooling process, Nd2Fe14B structure is formed, and finally the thin strip is broken into powder
Common applications of rare earth magnetic powder
computer hard drive
Wind Turbines
Speakers/Headphones
bicycle generator
MRI scanner
Industrial applications such as maintaining product purity, equipment protection and quality control
Contact Person: Jack Cui
Tel: 18653221706