Product Details:
|
Materail: | Anisotropic Bonded Samarium Iron Nitrogen Magnet | Application: | Industrial Magnet,Motor,Automotive,Customized |
---|---|---|---|
Grade: | MGT-IS-230,MGT-IS-240,MGT-IS-250,MGT-IS-260 | Size: | 1mm-100mm ,Customized |
Magetic Direction: | Axial,Radial,Skewed Angel Magnetized,Customized | Environment: | RoHs,Reach,SGS,MSDS |
Coating: | Uncoated,Customized | Color: | Black Or Brown Black |
High Light: | Samarium Iron Nitrogen Magnet,Anisotropic Bonded iron nitrogen magnet,Injection SmFeN Water Pump Magnet |
Anisotropic Bonded Samarium Iron Nitrogen Magnet Injection SmFeN Magnet Water Pump Magnet
Application
Feature
Anisotropic SmFeN+Ferrite(PA12) Compound for Injection | ||||||||||
HCSFY230L | HCSFY240L | HCSFY250L | HCSFY260L | HCSFY270L | HCSY280L | HCSY290L | ||||
单位Unit | SY+FY | SY+FY | SY+FY | SY+FY | SY+FY | SY | SY | |||
Magnetic Properties | Residual Induction | Br | mT | 330-370 | 400-490 | 500-540 | 540-580 | 590-630 | 500-600 | 570-680 |
kGs | 3.3-3.7 | 4.0-4.9 | 5.0-5.4 | 5.4-5.8 | 5.9-6.3 | 5.0-6.0 | 5.7-6.8 | |||
Coercive Force | Hcb | kA/m | 159-191 | 183-263 | 247-279 | 289-318 | 289-318 | 240-320 | 279-359 | |
kOe | 2.0-2.4 | 2.3-3.3 | 3.1-3.5 | 3.6-4.0 | 3.6-4.0 | 3.0-4.0 | 3.5-4.5 | |||
Intrinsic Coercivity | Hcj | kA/m | 223-303 | 350-517 | 398-438 | 430-462 | 438-494 | 240-560 | 340-640 | |
kOe | 2.8-3.8 | 4.4-6.5 | 5.0-5.5 | 5.4-5.8 | 5.5-6.2 | 3.0-7.0 | 4.0-8.0 | |||
Max.Product Energy | (BH)max | kJ/cm3 | 20-28 | 30-40 | 40-44 | 48-52 | 56-64 | 60-68 | 68-76 | |
MGOe | 2.5-3.5 | 4.0-5.0 | 5.0-5.5 | 6.0-6.5 | 7.0-8.0 | 7.5-8.5 | 8.5-9.5 | |||
Physical Properties | Density | ρ | g/cm3 | 3.5-3.9 | 3.6-4.0 | 3.8-4.2 | 4.0-4.3 | 4.1-4.4 | 3.8-4.3 | 4.0-4.5 |
Melt Flowrate | MFR | g/10min | 200-300 | 200-300 | 200-300 | 200-300 | 200-300 | 200-300 | 200-300 | |
(270℃ 10kg) | ||||||||||
Shrinkage | % | 0.6-1 | 0.6-1 | 0.6-1 | 0.6-1 | 0.6-1 | 0.6-1 | 0.6-1 | ||
Tensile Stength | ASTM-D638 | MPa | 45 | 46 | 47 | 48 | 49 | 45 | 45 | |
Flexural Modulus | ASTM-D790 | MPa | 75 | 78 | 80 | 85 | 86 | 75 | 75 | |
Flexural Modulus | ASTM-D790 | Gpa | 15 | 16 | 16 | 17 | 17 | 15 | 15 | |
IZOD Impact Strength | ASTM-D256 | (kJ/m2) | 7.8 | 8.2 | 8.4 | 8.1 | 8.1 | 7.8 | 7.8 | |
Injection Molding Process | ||||||||||
LT-35T (35ton ) Ring Φ10xΦ7x10 |
Predrying | ℃/hr | 80/4 | |||||||
Barrel Temp. | T1 | ℃ | 230 | 230 | 230 | 230 | 230 | 210 | 210 | |
T2 | ℃ | 245 | 245 | 245 | 245 | 245 | 230 | 230 | ||
T3 | ℃ | 250 | 250 | 250 | 250 | 250 | 235 | 235 | ||
Mold Temp. | ℃ | 80 | 80 | 80 | 80 | 80 | 80 | 80 | ||
Pressure | MPa (kg/cm2) |
105.8 (1079) |
105.8 (1079) |
105.8 (1079) |
105.8 (1079) |
105.8 (1079) |
117.5 (1199) |
117.5 (1199) |
||
Speed | % | 60 | 60 | 60 | 60 | 60 | 60 | 60 | ||
1. Molding conditions for customers'reference, the highest temperature of nylon injection barrel is not allowed to exceed 260 degrees. | ||||||||||
2. It can be customized according to customers'requirements |
Contact Person: Jack Cui
Tel: 18653221706